top of page
LCD Slimming Process OEM Service
(1) LCD slimming process OEM (thin processing / conductive film deposition)
At Renova Solutions, we perform the latter half process in the following LCD cell process.
TFT
CF
Cell
Inspection
Module
Washing
▼
Film formation
▼
Photolithography
▼
Fix
▼
Etching / peeling
BM formation
▼
Pigment application
▼
Photolithography
Alignment film formation
▼
Laminating / LCD
▼
Thin processing
(Slimming)
▼
Conductive (ITO) film formation
Cell division
▼
Lighting inspection
▼
Visual inspection
▼
Defect correction
IC connection
▼
Backlight
assembly
▼
Module
◆ Our thin processing (Slimming) adopts the most advanced Spray Down method.
Glass with a thickness of 1 mm or more is thinned to 0.2 mm by chemical treatment, and its uniformity is controlled by the thickness of one hair or less.
Contributes to weight reduction of smartphone or tablet displays etc..
Original plate glass
1500mm x 1800mm x thickness 1mm
SiO₂ + 6HF → H₂SiF₆ + 2H₂O etc.
After ultra-thin processing
0.2mm thick
◆ Shield-ITO
Achieves EMI countermeasures and external noise shielding while ensuring a transmittance of 96% or more.
(2) LCD packaging materials (exterior material / moisture absorbing material)
(3) FPD module process materials (AG paste / various resin materials / OCA, etc.)
Other Solution Business
Based on many years of close relationships with both domestic and oversea partners, we also are able to propose the up to date solutions for a series of various factory equipments. In order to improve our customer's technological development and productivity, operation and maintenance of equipment and facilities, ordering of suitable parts, selection of equipment models and process development service is available.