top of page

LCD Slimming Process OEM Service

Renova飛行機fav.png

(1) LCD slimming process OEM (thin processing / conductive film deposition)

​At Renova Solutions, we perform the latter half process in the following LCD cell process.

​TFT

CF

​Cell

 Inspection 

Module

Washing

Film formation

Photolithography

Fix

Etching / peeling

BM formation

Pigment application

Photolithography

Alignment film formation

Laminating / LCD

Thin processing

(Slimming)

Conductive (ITO) film formation

Cell division

Lighting inspection

Visual inspection

Defect correction

IC connection

Backlight
assembly

Module

◆ Our thin processing (Slimming) adopts the most advanced Spray Down method.
Glass with a thickness of 1 mm or more is thinned to 0.2 mm by chemical treatment, and its uniformity is controlled by the thickness of one hair or less.
Contributes to weight reduction of smartphone or tablet displaysetc..

1.png
2.png

Original plate glass

1500mm x 1800mm x thickness 1mm

SiO₂ + 6HF → H₂SiF₆ + 2H₂O etc.

After ultra-thin processing

0.2mm thick

0.2㎜.png
ITO.png

◆ Shield-ITO

Achieves EMI countermeasures and external noise shielding while ensuring a transmittance of 96% or more.

(2) LCD packaging materials (exterior material / moisture absorbing material)
(3) FPD module process materials (AG paste / various resin materials / OCA, etc.)

Other ​Solution Business

Based on many years of close relationships with both domestic and oversea partners, we also are able to propose the up to date solutions for a series of various factory equipments.  In order to improve our customer's technological development and productivity, operation and maintenance of equipment and facilities, ordering of suitable parts, selection of equipment models and process development service is available.